Polyester Rolls 

Film Polyester Class B (130°C)

Excellent resistance to chemicals; diluted acids, current impregnation varnishes. Low resistance to concentrated acids, phenols.

 

Table 1 - Main Characteristics Class B 130ºC.

Properties

Values

Units

Observations

Density  1,39 g/cm³ -
Water Absorption < 0,6 % 24 hours in water
Film 25  24 g/m²/24h Film 25 μ 39,5 ºC - 100 HR
O2 Permeability 40 cm³/m²/24h Film 25 μ - 20 ºC
Refractive Index 1.64 nD 25  à 23 ºC
Tensile Strength 1.900 kg/cm² Film < 25 μ
1.600 kg/cm² Film > 25 μ
Elongation 60 à 80 % Film < 25 μ
100 à 140 % Film > 25 μ
Tear Strength  18 à 20 g Elmendorf on film 25 μ
Bursting Strength > 5 kg/cm² 25 Film < 25 μ thick (Lhomargy)
Folding resistance > 20 000 Pliages Film 25 μ
Dard test 400 grammes Film 25 μ
Melting point 250 -255 ºC  
Shrinkage 1 to 3 % at 150 ºC (30 minutes)
Thermal conductivity 3,63 X 10 (-4) cal/sec/ºC -
Thermal class (continuous usage) -60 + 140 ºC -

 

 

Table 2 - Main Characteristics Class B 130ºC.

Properties

Test Conditions

Results

Units 
Dielectric strength 50 Hz sur 25 ºC 180.00 Volts/mm
 film 50 μ 150 ºC 126.00
Dielectric constant

50 Hz{

25 ºC 3.0/3.1 -
90 ºC 3.2/3.3
150 ºC 3.7

25 ºC{

50 Hz 3.0/3.1
1 K Hz 2.9/3.1
1 M Hz 2.8/3.00
Dissipation factor (tg delta) 

50 Hz{

25 ºC 2 x 10 -³ -
150 Hz 5 x 10 -³

25 ºC{

50 Hz 2 x 10 -³
1 K Hz 6 x 10 -³
1 M Hz 20 x 10 -³
Volume resistivity  - 25 ºC 1 x 10 -17 Ohm. cm
90 ºC 4 x 10 -16
150 ºC 1 x 10 -13
Surface resistivity 25 ºC-50 % hR - 1 à 5  x 10 -14 Ohm. cm/cm
Insulation resistivity 130 ºC s/condens. 0.5 μF  800 - 1.00 M Ohm. μF
150 ºC on/capacitors. 0.5 μF  8 - 100
The above values are typical and are only intended to be used as a guide.

 

 

Copyright © 1999 E. C. Menzies Electrical Pty Ltd
Use of this site indicates you accept the Terms of Use
Contact us by email at Sales, or for web site issues contact Web Master
Last modified: June 29, 2001